# The effect of holding time on nanoindentation measurements of creep in bone

**Type:** Papers  
**Canonical URL:** https://scholariq.org/papers/the-effect-of-holding-time-on-nanoindentation-measurements-of-creep-in-bone/

## Facts

| Field | Value |
| --- | --- |
| Author Names | Ziheng Wu,Tyler A. Baker,Timothy C. Ovaert,Glen L. Niebur |
| Citations | 75 |
| DOI | 10.1016/j.jbiomech.2011.01.039 |
| Fields | Engineering,Materials Science |
| Open Access | false |
| OA Status | closed |
| OpenAlex ID | https://openalex.org/W2084324168 |
| PMID | 21353675 |
| Type | article |
| Year | 2011 |

## Paper authors

- [Ziheng Wu](https://scholariq.org/researchers/ziheng-wu/)

## Paper journal

- [Journal of Biomechanics](https://scholariq.org/journals/journal-of-biomechanics/)

## Paper primary topic

- [Metal and Thin Film Mechanics](https://scholariq.org/topics/metal-and-thin-film-mechanics/)

## Paper topics

- [Metal and Thin Film Mechanics](https://scholariq.org/topics/metal-and-thin-film-mechanics/)
- [Diamond and Carbon-based Materials Research](https://scholariq.org/topics/diamond-and-carbon-based-materials-research/)
- [Advanced materials and composites](https://scholariq.org/topics/advanced-materials-and-composites/)

---
Source: ScholarIQ — public research metadata, principally OpenAlex. See https://scholariq.org/sources/ for provenance and https://scholariq.org/methodology/ for what these figures mean.